Process for Cleaning and Polishing Cobalt/Chromium |
|
|
|
 Minimum recommended process for electropolishing Cobalt/Chromium
This is effective ONLY with metal which does not contain colored oxide:
Step |
Process Line / Description |
1. |
|
2.
| Water Rinse |
3.
| Alcohol Rinse |
4.
| |
This process is effective for metal which has colored oxide:
Step |
Process Line |
Concentration & Temperature |
Equipment Required |
Ventilation Requirements |
1. |
|
100% 50°+ C |
SS labware PP or PVC |
Not Required |
2. |
Rinse in tap water |
|
|
3. |
|
50% Part A 50% Part B 80°–100° C 4-24 hours |
Pyrex or SS |
Not Required |
4. |
Rinse in tap water |
Room Temperature |
|
5. |
|
100% Room Temp 60 Seconds |
Glass or Plastic |
Recommended |
6. |
Rinse in tap water |
|
|
7. |
Rinse in dry alcohol |
|
|
??? |
8. |
|
100% Room Temperature |
SS |
Required |
9. |
Rinse in water |
|
|
|